Moulin Fritte M1511

Fritte Boro-acaline Plombeuse

OxideAnalysisFormula
BaO23.10%0.314
Na2O10.20%0.342
PbO36.90%0.344
SiO229.80%1.032
Oxide Weight208.11
Formula Weight208.11
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 504C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Moulin Fritte M1511" descrip="Fritte Boro-acaline Plombeuse" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="23.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.200" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="36.900" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="29.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved