Molybdenum Trioxide

Formula: MoO3

OxideAnalysisFormula
MoO3100.00%1.000
Oxide Weight143.94
Formula Weight143.94
If this formula is not unified correctly please contact us.

Lowers surface tension of melts and thus can be used to encourage crystal development (i.e. with titanium), variegate colorants, impart silvery coloration, opacify. Also used in yellow stains and as a color stabilizer and in lustres to add gold coloration. It is generally a weak influence in these areas.

MoO3 can varporize and have effects on other glazes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Molybdenum Trioxide" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="MoO3" name="Molybdic Oxide" status="" percent="100.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved