Molybdenum Disulfide

Formula: MoS2

OxideAnalysisFormula
MoO389.88%1.000
LOI10.12
Oxide Weight143.94
Formula Weight160.15
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Molybdenum Disulfide" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="MoO3" name="Molybdic Oxide" status="" percent="89.880" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="10.120" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved