MOK 3 Borax frit

Low melting high expansion frit

Alternate Names: Frit MOK Boraksfritte, Frit G-3

OxideAnalysisFormula
MgO0.04%0.003
K2O9.52%0.338
Na2O12.21%0.659
Al2O39.88%0.324
B2O314.86%0.714
SiO253.49%2.977
Oxide Weight334.46
Formula Weight334.46
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 780-1000

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="MOK 3 Borax frit" descrip="Low melting high expansion frit" searchkey="Frit MOK Boraksfritte, Frit G-3" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.040" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="9.520" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="12.210" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.880" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.860" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.490" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved