Miyoomizan Feldspar

OxideAnalysisFormula
CaO0.87%0.103
MgO0.06%0.010
K2O5.01%0.353
Na2O4.99%0.534
P2O50.01%0.000
TiO20.04%0.003
Al2O318.01%1.171
SiO269.97%7.724
Fe2O30.19%0.008
LOI0.85
Oxide Weight657.77
Formula Weight663.41
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Miyoomizan Feldspar" descrip="" searchkey="" loi="0.85" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.870" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.060" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.010" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.990" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.010" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.040" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="18.010" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="69.970" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.190" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.850" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved