Mikumo Feldspar

OxideAnalysisFormula
CaO0.54%0.075
MgO0.02%0.004
K2O4.80%0.399
Na2O3.30%0.417
P2O50.01%0.001
TiO20.04%0.004
Al2O313.02%1.000
SiO277.39%10.088
Fe2O30.21%0.010
LOI0.67
Oxide Weight778.16
Formula Weight783.41
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Mikumo Feldspar" descrip="" searchkey="" loi="0.67" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.540" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.020" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.300" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.010" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.040" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="13.020" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="77.390" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.210" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.670" tolerance=""/> </volatiles> </material>