Matthey Frit 21065g

GLAZE LEAD BORAX

OxideAnalysisFormula
CaO6.06%0.380
K2O0.80%0.030
Na2O5.11%0.290
PbO19.03%0.300
Al2O37.83%0.270
B2O37.52%0.380
SiO253.65%3.141
Oxide Weight351.87
Formula Weight351.87
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.4 x 10-6

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Matthey Frit 21065g" descrip="GLAZE LEAD BORAX" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.060" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.800" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.110" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="19.030" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.830" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="7.520" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="53.650" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved