Matthey Frit 20306G

Calcium boro silicate frit

OxideAnalysisFormula
CaO10.66%0.666
K2O0.54%0.020
Na2O5.54%0.313
Al2O313.51%0.465
B2O313.23%0.667
SiO256.51%3.298
Oxide Weight350.71
Formula Weight350.71
If this formula is not unified correctly please contact us.

Calculated raw sub:
Gerstely Borate 19.5
Pioneer Kaolin 15.0
Flint 25.0
Whiting 8.5
Nepheline Syenite 19


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Matthey Frit 20306G" descrip="Calcium boro silicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.660" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.540" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="5.540" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.510" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.230" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.510" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved