M136

Natriubor-Silikat

Alternate Names: M 136,M-136

OxideAnalysisFormula
CaO0.45%0.690
K2O0.15%0.137
PbO0.45%0.173
Al2O30.15%0.126
B2O30.45%0.556
SiO21.75%2.504
Oxide Weight292.35
Formula Weight292.35
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 67
GSPT - Frit Softening Point 603C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="M136" descrip="Natriubor-Silikat" searchkey="M 136,M-136" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.450" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.150" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="0.450" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.150" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="0.450" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="1.750" tolerance=""/> </oxides> </material>