Luzenac Talc 00S

Alternate Names: Talc OOS, OOS Talc

OxideAnalysisFormula
CaO0.30%0.007
MgO31.90%0.993
TiO20.10%0.002
Al2O32.80%0.034
SiO257.80%1.207
Fe2O30.80%0.006
LOI6.20
Oxide Weight117.58
Formula Weight125.35
If this formula is not unified correctly please contact us.

Chemistry from Solargil website, 2008


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Luzenac Talc 00S" descrip="" searchkey="Talc OOS, OOS Talc" loi="0.00" casnumber="14807-96-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="31.900" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.100" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.800" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.800" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="6.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved