Lead Oxide and Lead Orthosilicate Eutectic

OxideAnalysisFormula
PbO91.70%1.000
SiO28.30%0.336
Oxide Weight243.40
Formula Weight243.40
If this formula is not unified correctly please contact us.
GSPT - Frit Softening Point 552C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Lead Oxide and Lead Orthosilicate Eutectic" descrip="" searchkey="" loi="0.00" casnumber="n/a"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="91.700" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="8.300" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved