Lead Bisilcate B-15

Lead alumina bilsilicate frit (with 1% TiO2)

OxideAnalysisFormula
PbO63.00%1.000
TiO21.00%0.044
Al2O32.00%0.069
SiO234.00%2.004
Oxide Weight354.29
Formula Weight354.29
If this formula is not unified correctly please contact us.
DENS - Density (Specific Gravity) 4.65-4.95
MLRG - Frit Melting Range (C) 788-816C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Lead Bisilcate B-15" descrip="Lead alumina bilsilicate frit (with 1% TiO2)" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="63.000" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="2.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="34.000" tolerance=""/> </oxides> </material>