OxideAnalysisFormula
CaO18.90%0.712
MgO2.30%0.121
K2O1.40%0.031
Na2O4.00%0.136
Al2O38.10%0.168
B2O327.50%0.835
SiO218.70%0.657
Fe2O30.10%0.001
LOI19.00
Oxide Weight171.12
Formula Weight211.26
If this formula is not unified correctly please contact us.

A specially formulated flux containing a high percentage of boron. This material mimics the fluxing characteristics of Gerstley Borate.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Laguna Borate" descrip="Gerstley Borate Alternative" searchkey="" loi="0.00" casnumber="167077-83-0"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="18.900" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="2.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.100" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="27.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="18.700" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.100" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="19.000" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved