Kurts Corn Stn

A material from Ron Roys MDT

OxideAnalysisFormula
BaO0.01%0.000
CaO1.51%0.206
MgO0.10%0.019
K2O4.10%0.333
Na2O3.37%0.416
P2O50.48%0.026
TiO20.05%0.005
Al2O316.67%1.250
SiO271.61%9.115
Fe2O30.18%0.009
LOI1.91
Oxide Weight750.28
Formula Weight764.89
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kurts Corn Stn" descrip="A material from Ron Roys MDT" searchkey="" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.010" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.510" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.100" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="4.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.370" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.480" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.050" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="16.670" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="71.610" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.180" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="1.910" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved