Kuncice Dolomite

Unknown

OxideAnalysisFormula
CaO32.00%0.534
MgO19.90%0.462
K2O0.40%0.004
Al2O30.30%0.003
SiO21.30%0.020
LOI46.00
Oxide Weight50.45
Formula Weight93.42
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kuncice Dolomite" descrip="Unknown" searchkey="" loi="0.00" casnumber="69598-19-2"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="32.000" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="19.900" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.400" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="0.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="1.300" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="46.000" tolerance=""/> </volatiles> </material>