Keramikos Fritte M1

Borax Fritte

OxideAnalysisFormula
BaO2.92%0.048
CaO11.69%0.525
MgO0.43%0.027
K2O1.61%0.043
Na2O8.79%0.357
B2O317.33%0.627
SiO257.34%2.403
Oxide Weight252.19
Formula Weight252.19
If this formula is not unified correctly please contact us.
MLRG - Frit Melting Range (C) 850-1060C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Fritte M1" descrip="Borax Fritte" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="2.920" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.690" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.430" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.610" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="8.790" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="17.330" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.340" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved