Keramikos Fritte 32.22

Zink Fritte, Zinc frit

OxideAnalysisFormula
CaO2.98%0.097
K2O5.00%0.097
Na2O4.94%0.146
ZnO29.38%0.660
B2O311.45%0.301
SiO246.25%1.407
Oxide Weight182.88
Formula Weight182.88
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Fritte 32.22" descrip="Zink Fritte, Zinc frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.980" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="5.000" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.940" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="29.380" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="11.450" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.250" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved