Keramikos Fritte 31.10

Natriumsilicaat Fritte, sodium frit

Alternate Names: CH179E

OxideAnalysisFormula
CaO6.28%0.293
K2O2.18%0.061
Na2O15.31%0.646
Al2O33.54%0.091
B2O32.42%0.091
SiO270.27%3.061
Oxide Weight261.77
Formula Weight261.77
If this formula is not unified correctly please contact us.

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Fritte 31.10" descrip="Natriumsilicaat Fritte, sodium frit" searchkey="CH179E" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.280" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.180" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="15.310" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.540" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="2.420" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.270" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved