Keramikos Fritte 15.11

Natriumloodboor Fritte

Oxide Weight302.40
Formula Weight302.40
If this formula is not unified correctly please contact us.

Out Bound Links

By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Fritte 15.11" descrip="Natriumloodboor Fritte" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="10.250" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="36.910" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="23.020" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="29.820" tolerance=""/> </oxides> </material>