OxideAnalysisFormula
CaO2.81%0.100
K2O2.83%0.060
Na2O19.23%0.620
ZnO8.96%0.220
Al2O33.06%0.060
SiO263.12%2.099
Oxide Weight199.87
Formula Weight199.87
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Fritte 15.10" descrip="Alkali Fritte" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.810" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.830" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="19.230" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="8.960" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="3.060" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.120" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved