Keramikos Fritte 10.01

Lead Monosilicate frit, Loodmonosilicaat Fritte

OxideAnalysisFormula
PbO78.92%1.000
SiO221.71%1.022
Oxide Weight284.60
Formula Weight284.60
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Fritte 10.01" descrip="Lead Monosilicate frit, Loodmonosilicaat Fritte" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="78.920" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="21.710" tolerance=""/> </oxides> </material>