Keramikos Bariumzink Fritte

Barium zinc frit

OxideAnalysisFormula
BaO35.63%0.500
ZnO18.92%0.500
Al2O35.22%0.110
SiO240.23%1.440
Oxide Weight215.12
Formula Weight215.12
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Bariumzink Fritte" descrip="Barium zinc frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="35.630" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="18.920" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.220" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="40.230" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved