Keramikos Aardalkaliboor Fritte

High potassium sodium frit

OxideAnalysisFormula
CaO2.74%0.100
K2O20.73%0.450
Na2O13.64%0.450
Al2O39.98%0.200
SiO252.90%1.800
Oxide Weight204.52
Formula Weight204.52
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Keramikos Aardalkaliboor Fritte" descrip="High potassium sodium frit" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="2.740" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="20.730" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="13.640" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="9.980" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.900" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved