Kaolin 171

Alternate Names: Kaolen 171

OxideAnalysisFormula
CaO0.26%0.013
MgO0.62%0.044
K2O0.12%0.004
Na2O0.20%0.009
TiO20.28%0.010
Al2O335.55%1.000
SiO246.87%2.238
Fe2O31.90%0.034
SO40.38
LOI14.20
Oxide Weight246.18
Formula Weight288.20
If this formula is not unified correctly please contact us.

Available in minus 20cm, -100 microns, -75 microns.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kaolin 171" descrip="" searchkey="Kaolen 171" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.260" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.620" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.120" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.280" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="35.550" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="46.870" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.900" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="0.380" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="14.200" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved