Kaolin 151

Alternate Names: Kaolen 151

OxideAnalysisFormula
CaO0.26%0.013
MgO0.17%0.012
K2O0.13%0.004
Na2O0.06%0.003
TiO20.22%0.008
Al2O335.75%1.000
SiO245.31%2.151
Fe2O30.75%0.013
SO40.34
LOI16.42
Oxide Weight235.81
Formula Weight283.29
If this formula is not unified correctly please contact us.

Available in minus 20cm, -100 microns, -75 microns.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kaolin 151" descrip="" searchkey="Kaolen 151" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.260" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.170" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.130" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.060" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.220" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="35.750" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.310" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.750" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="0.340" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="16.420" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved