•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

Kaolin 143

Alternate Names: Kaolen 143

OxideAnalysisFormula
CaO0.34%0.017
MgO0.19%0.014
K2O0.12%0.004
Na2O0.09%0.004
TiO20.23%0.008
Al2O335.41%1.000
SiO249.90%2.392
Fe2O30.66%0.012
SO40.52
LOI12.57
Oxide Weight250.43
Formula Weight288.15
If this formula is not unified correctly please contact us.
DS - Dry Strength (kgf/cm2) 12.14
WABS - Water absorption 1100C: 20% 1200C: 18 1250C: 18 1325C: 15
FSHR - Firing Shrinkage 1150C: 3.0% 1200C: 5.0 1250C: 5.1 1325C: 5.5

Available in run-of-mine, 25mm and 50mm sizes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kaolin 143" descrip="" searchkey="Kaolen 143" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.340" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.190" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.120" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.090" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.230" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="35.410" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.660" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="0.520" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="12.570" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved