Kaolin 114

Alternate Names: Kaolen 114

OxideAnalysisFormula
CaO0.25%0.017
MgO0.24%0.023
K2O0.40%0.016
Na2O0.38%0.024
TiO20.35%0.017
Al2O326.50%1.000
SiO260.16%3.853
Fe2O30.82%0.020
SO40.71
LOI10.90
Oxide Weight342.95
Formula Weight388.00
If this formula is not unified correctly please contact us.
WABS - Water absorption 1000C: 20.5% 1100C: 19.5% 1200C: 17.7% 1250C: 17%
FSHR - Firing Shrinkage 1000C: 7.5% 1100C: 9% 1200C: 9.5% 1250C: 10.5%

Available in run-of-mine, 25mm and 50mm sizes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kaolin 114" descrip="" searchkey="Kaolen 114" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.250" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.240" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.380" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.350" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="26.500" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="60.160" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.820" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="0.710" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="10.900" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved