Kaolin 113

Alternate Names: Kaolen 113

OxideAnalysisFormula
CaO0.20%0.017
MgO0.07%0.008
K2O0.04%0.002
Na2O0.09%0.007
TiO20.33%0.020
Al2O321.31%1.000
SiO270.24%5.594
Fe2O30.48%0.014
SO40.52
LOI7.24
Oxide Weight443.99
Formula Weight481.35
If this formula is not unified correctly please contact us.
WABS - Water absorption 1000C: 19.3% 1100C: 18.3% 1200C: 17.5% 1250C: 17%
FSHR - Firing Shrinkage 1000C: 7.3% 1100C: 7.5% 1200C: 7.8% 1250C: 7.9%

Available in run-of-mine, 25mm and 50mm sizes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kaolin 113" descrip="" searchkey="Kaolen 113" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.070" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.040" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.090" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.330" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="21.310" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="70.240" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.480" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="0.520" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="7.240" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved