Kaolin 111

Alternate Names: Kaolen 111

OxideAnalysisFormula
CaO0.28%0.033
MgO0.19%0.031
K2O0.04%0.003
Na2O0.04%0.004
TiO20.30%0.025
Al2O315.33%1.000
SiO277.35%8.563
Fe2O30.52%0.022
SO40.40
LOI5.95
Oxide Weight625.77
Formula Weight668.20
If this formula is not unified correctly please contact us.
WABS - Water absorption 1000C: 23% 1100C: 22.5 1200C: 22% 1250C: 21.8%
FSHR - Firing Shrinkage 1000C: 6.7% 1100C: 6.8% 1200C: 6.9% 1250C: 7.0%

Available in run-of-mine, 25mm and 50mm sizes.


Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kaolin 111" descrip="" searchkey="Kaolen 111" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.280" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.190" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.040" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.040" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.300" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="15.330" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="77.350" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.520" tolerance=""/> </oxides> <volatiles> <volatile symbol="SO4" name="Sulfate" percent="0.400" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="5.950" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved