Kaolex D-6 Kaolin

OxideAnalysisFormula
TiO21.50%0.049
Al2O339.00%1.000
SiO245.90%1.997
Fe2O30.60%0.010
LOI13.32
Oxide Weight227.54
Formula Weight262.50
If this formula is not unified correctly please contact us.
PCE - Pyrometric Cone Equivalent 34-35

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Kaolex D-6 Kaolin" descrip="" searchkey="" loi="0.00" casnumber="95077-05-7"> <oxides> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="39.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="45.900" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="13.320" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved