•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

K-200 Feldspar

POTASSIUM/SODIUM/CALCIUM FELDSPAR

Alternate Names: K200 Feldspar

OxideAnalysisFormula
CaO0.18%0.019
K2O10.13%0.652
Na2O3.36%0.329
Al2O317.84%1.060
SiO267.99%6.859
Fe2O30.08%0.003
LOI0.31
Oxide Weight603.74
Formula Weight605.61
If this formula is not unified correctly please contact us.

K-200 is a high quality feldspar ground to 200 mesh for ceramic applications. It has one of the highest potassium contents of any spar. Carefully beneficiated and controlled for quality, K-200 offers high potash content and low iron oxide per unit of alumina.

Sieve Analysis (Cum):
+200 mesh: 0.3%
+325 mesh: 3.2%

Average Particle Size: 10.1 microns
Specific Surface Area: 1.88 square meters per gram
Bulk Density: 62 lbs/cu ft loose, 74 packed


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="K-200 Feldspar" descrip="POTASSIUM/SODIUM/CALCIUM FELDSPAR" searchkey="K200 Feldspar" loi="0.00" casnumber="12168-80-8"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.180" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="10.130" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.360" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.840" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="67.990" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="0.080" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="0.310" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved