Jasper Red

OxideAnalysisFormula
MgO0.23%0.034
K2O0.71%0.045
Na2O0.23%0.022
TiO21.69%0.125
Al2O317.26%1.000
SiO263.05%6.200
Fe2O38.43%0.311
LOI8.40
Oxide Weight541.32
Formula Weight590.96
If this formula is not unified correctly please contact us.

A very red burning medium to low plasticity stoneware clay useful in both plastic and casting bodies. Crude color is red-brown.

Shrinkage:
Cone 05: 6%
Cone 1: 9%
Cone 5: 10%
Cone 10: 11-12%

Absorption:
Cone 05: 19%
Cone 1: 13%
Cone 5: 12%
Cone 10: 8%

+200 mesh residue Wet: 9.5%
PCE: 14
M.O.R.: 274 psi


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Jasper Red" descrip="" searchkey="" loi="8.40" casnumber=""> <oxides> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.230" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.710" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.230" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.690" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="U" percent="17.260" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="63.050" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="8.430" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="8.400" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved