James Kent Frit SN72

TRANSPARENT (FORMERLY #FTO517)

OxideAnalysisFormula
CaO14.00%0.530
KNaO7.00%0.190
ZnO18.00%0.470
Al2O312.00%0.250
SiO249.00%1.732
Oxide Weight212.46
Formula Weight212.46
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 0.423 @ 500C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="James Kent Frit SN72" descrip="TRANSPARENT (FORMERLY #FTO517)" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="14.000" tolerance=""/> <oxide symbol="KNaO" name="Potassium/Sodium Oxides" status="" percent="7.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="18.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="49.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved