James Kent Frit SN70

OPAQUE (FORMERLY #90401034)

OxideAnalysisFormula
CaO6.00%0.813
KNaO8.00%0.779
ZnO2.00%0.187
Al2O38.00%0.596
B2O312.00%1.311
SiO254.00%6.832
ZrO28.00%0.494
Oxide Weight745.12
Formula Weight745.12
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 0.291 @ 500C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="James Kent Frit SN70" descrip="OPAQUE (FORMERLY #90401034)" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.000" tolerance=""/> <oxide symbol="KNaO" name="Potassium/Sodium Oxides" status="" percent="8.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="2.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="12.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="54.000" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="8.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved