James Kent Frit N4129

TRANSPARENT (FORMERLY #90400023)

OxideAnalysisFormula
CaO12.00%1.000
KNaO10.00%0.599
Al2O35.00%0.229
B2O320.00%1.343
SiO252.00%4.045
Oxide Weight462.83
Formula Weight462.83
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 0.399 @ 500C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="James Kent Frit N4129" descrip="TRANSPARENT (FORMERLY #90400023)" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.000" tolerance=""/> <oxide symbol="KNaO" name="Potassium/Sodium Oxides" status="" percent="10.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="20.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="52.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved