James Kent Frit DR1327

Zinc barium calcium alkali frit (formerly #FT0540)

OxideAnalysisFormula
BaO3.00%0.058
CaO11.00%0.579
KNaO9.00%0.340
ZnO10.00%0.363
Al2O38.00%0.232
B2O36.00%0.255
SiO256.00%2.753
Oxide Weight304.29
Formula Weight304.29
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 0.335 @ 500C

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="James Kent Frit DR1327" descrip="Zinc barium calcium alkali frit (formerly #FT0540)" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="3.000" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="11.000" tolerance=""/> <oxide symbol="KNaO" name="Potassium/Sodium Oxides" status="" percent="9.000" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="10.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="8.000" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="6.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.000" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved