JAE Vit R Ball Clay

Thailand Ball Clay

OxideAnalysisFormula
CaO0.30%0.023
MgO1.30%0.139
K2O2.40%0.110
Na2O0.80%0.056
TiO20.70%0.038
Al2O323.60%1.000
SiO258.80%4.229
Fe2O31.60%0.043
C0.10
LOI6.40
Oxide Weight386.82
Formula Weight413.71
If this formula is not unified correctly please contact us.

Particle Size (e.s.d.)
125 microns - 1.0
20 microns - 99
2 microns - 74
.5 microns - 48
Modulus of Rupture at 110C
Mn/M2 - 7.8
lbf/in2 - 1130
Water Absorption
1120C - 0.0
1220C - 0.5
Shrinkage Dry to Fired
1120C - 11.5
1220C - 8.5


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="JAE Vit R Ball Clay" descrip="Thailand Ball Clay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.300" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.300" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.400" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.800" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.700" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="23.600" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.600" tolerance=""/> </oxides> <volatiles> <volatile symbol="C" name="Carbon" percent="0.100" tolerance=""/> <volatile symbol="LOI" name="Loss on Ignition" percent="6.400" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved