IXL 45F

IRON BEARING SANDY CLAY

OxideAnalysisFormula
CaO1.68%0.257
MgO1.49%0.317
K2O2.76%0.251
Na2O1.26%0.174
TiO20.29%0.032
Al2O313.41%1.128
SiO272.73%10.384
Fe2O33.58%0.192
LOI3.50
Oxide Weight834.08
Formula Weight864.33
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="IXL 45F" descrip="IRON BEARING SANDY CLAY" searchkey="" loi="3.50" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="1.680" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="1.490" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.760" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.260" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.295" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="13.410" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="72.730" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="3.580" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="3.500" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved