IXL 45D

TAN BROWN BURNING MIDDLE STONEWARE

OxideAnalysisFormula
CaO0.37%0.039
MgO0.83%0.123
K2O3.60%0.228
Na2O0.70%0.067
P2O50.15%0.006
TiO20.66%0.049
Al2O317.10%1.000
SiO266.10%6.560
Fe2O32.19%0.082
MnO0.00%0.001
LOI6.70
Oxide Weight547.04
Formula Weight586.32
If this formula is not unified correctly please contact us.

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="IXL 45D" descrip="TAN BROWN BURNING MIDDLE STONEWARE" searchkey="" loi="6.70" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.370" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.830" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.600" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.700" tolerance=""/> <oxide symbol="P2O5" name="Phosphorus Pentoxide" status="" percent="0.150" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="0.663" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="17.100" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="66.100" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.190" tolerance=""/> <oxide symbol="MnO" name="Manganous Oxide" status="" percent="0.006" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="6.700" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved