Cedar Heights Fireclay

OxideAnalysisFormula
CaO0.20%0.013
MgO0.40%0.037
K2O2.10%0.083
Na2O0.20%0.012
TiO21.50%0.070
Al2O327.30%1.000
SiO257.80%3.593
Fe2O31.70%0.040
H2O8.80
Oxide Weight340.75
Formula Weight373.63
If this formula is not unified correctly please contact us.
PCE - Pyrometric Cone Equivalent 29

Medium buff burning fireclay available in 12 and 30 mesh sizes.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Industrial Fireclay" descrip="Cedar Heights Fireclay" searchkey="" loi="0.00" casnumber="70694-09-6"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.200" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.400" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.200" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.500" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="27.300" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="57.800" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.700" tolerance=""/> </oxides> <volatiles> <volatile symbol="H2O" name="Water" percent="8.800" tolerance=""/> </volatiles> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved