•The secret to cool bodies and glazes is a lot of testing.
•The secret to know what to test is material and chemistry knowledge.
•The secret to learning from testing is documentation.
•The place to test, do the chemistry and document is an account at https://insight-live.com
•The place to get the knowledge is https://digitalfire.com

Sign-up at https://insight-live.com today.

IMCO KPW Clay

OxideAnalysisFormula
CaO0.02%0.001
MgO0.47%0.047
K2O3.20%0.137
Na2O0.16%0.010
TiO21.04%0.053
Al2O325.20%1.000
SiO261.20%4.122
Fe2O31.74%0.044
LOI11.00
Oxide Weight376.55
Formula Weight423.09
If this formula is not unified correctly please contact us.

Manufacturer says: A nice white clay in the raw state. Fires to a cream color.

Physical data can be found on the link to the product information web page of the manufacturer.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="IMCO KPW Clay" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.020" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.470" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="3.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="0.160" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.040" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="25.200" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="61.200" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="1.740" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="11.000" tolerance=""/> </volatiles> </material>