IMCO Howard Clay

OxideAnalysisFormula
CaO0.22%0.014
MgO0.44%0.038
K2O0.57%0.021
TiO21.68%0.074
Al2O329.00%1.000
SiO248.50%2.838
Fe2O32.24%0.049
LOI16.00
Oxide Weight290.70
Formula Weight346.07
If this formula is not unified correctly please contact us.

Howard Clay is a highly plastic fire clay with low free silica. It is used in many types of ceramic and industrial applications.

Physical data can be found on the link to the product information web page of the manufacturer.


Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="IMCO Howard Clay" descrip="" searchkey="" loi="0.00" casnumber=""> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="0.220" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.440" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="0.570" tolerance=""/> <oxide symbol="TiO2" name="Titanium Dioxide, Titania" status="" percent="1.680" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="29.000" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="48.500" tolerance=""/> <oxide symbol="Fe2O3" name="Iron Oxide, Ferric Oxide" status="" percent="2.240" tolerance=""/> </oxides> <volatiles> <volatile symbol="LOI" name="Loss on Ignition" percent="16.000" tolerance=""/> </volatiles> </material>