1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Idaho 1 Fireclay

Alternate Names: Idaho I Fireclay, A.P. Green Idaho 1

Oxide Analysis Formula
CaO 0.48% 0.02
K2O 0.31% 0.01
MgO 0.26% 0.02
Na2O 0.31% 0.01
TiO2 1.13% 0.04
Al2O3 35.39% 1.00
SiO2 46.96% 2.25
Fe2O3 1.29% 0.02
LOI13.87%
Oxide Weight 248.24
Formula Weight 288.22

Related Information

Links

Materials Fireclay
Suppliers A. P. Green
Typecodes Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service.
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

By Tony Hansen


Tell Us How to Improve This Page

Or ask a question and we will alter this page to better answer it.

Email Address

Name

Subject

Message


Upload picture


Copyright 2008, 2015, 2017 https://digitalfire.com, All Rights Reserved