Hommel Frit 698

Zircon borosilicate frit

OxideAnalysisFormula
CaO6.03%0.494
Na2O6.06%0.449
ZnO1.00%0.056
Al2O34.16%0.188
B2O313.63%0.900
SiO256.72%4.339
ZrO212.38%0.462
Oxide Weight459.65
Formula Weight459.65
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 6.00
GSPT - Frit Softening Point 1720F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 698" descrip="Zircon borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.030" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="6.060" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="1.000" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="4.160" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="13.630" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="56.720" tolerance=""/> <oxide symbol="ZrO2" name="Zirconium Dioxide" status="" percent="12.380" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved