Hommel Frit 584

Lead monoborate frit

OxideAnalysisFormula
PbO85.24%1.000
B2O314.76%0.555
Oxide Weight261.85
Formula Weight261.85
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 12.00
GSPT - Frit Softening Point 800F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 584" descrip="Lead monoborate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="PbO" name="Lead Oxide" status="" percent="85.240" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="14.760" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved