Hommel Frit 576

Calcium borosilicate very low lead frit

OxideAnalysisFormula
CaO6.92%0.629
K2O1.10%0.060
Na2O2.81%0.231
PbO3.49%0.080
Al2O35.61%0.281
B2O324.21%1.775
SiO255.86%4.742
Oxide Weight510.24
Formula Weight510.24
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 5.4 x 10-6
GSPT - Frit Softening Point 1465F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 576" descrip="Calcium borosilicate very low lead frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="6.920" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="1.100" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.810" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="3.490" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.610" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="24.210" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.860" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved