Hommel Frit 573

High lead zinc frit

OxideAnalysisFormula
Na2O1.20%0.037
ZnO19.75%0.469
PbO57.05%0.494
Al2O31.96%0.037
SiO220.03%0.644
Oxide Weight193.19
Formula Weight193.19
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 10.6 x 10-6
GSPT - Frit Softening Point 1560F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 573" descrip="High lead zinc frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="1.200" tolerance=""/> <oxide symbol="ZnO" name="Zinc Oxide" status="" percent="19.750" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="57.050" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="1.960" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="20.030" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved