Hommel Frit 494

Leadless strontium barium frit

OxideAnalysisFormula
BaO11.20%0.200
CaO9.35%0.457
MgO0.41%0.028
K2O2.20%0.064
Na2O2.03%0.090
SrO6.08%0.161
Al2O35.09%0.137
B2O37.99%0.315
SiO255.66%2.540
Oxide Weight274.24
Formula Weight274.24
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 8.00

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 494" descrip="Leadless strontium barium frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="11.200" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="9.350" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.410" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.200" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="2.030" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="6.080" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="5.090" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="7.990" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="55.660" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved