Hommel Frit 488

OxideAnalysisFormula
BaO17.81%0.217
CaO12.16%0.406
K2O12.01%0.239
Na2O4.59%0.139
Al2O310.83%0.199
SiO242.60%1.326
Oxide Weight187.10
Formula Weight187.10
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 11.7 x 10-6
MLRG - Frit Melting Range (C) 1580F

Out Bound Links

In Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 488" descrip="" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="17.810" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="12.160" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="12.010" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="4.590" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="10.830" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="42.600" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved