Hommel Frit 486

Calcium strontium borosilicate frit

OxideAnalysisFormula
BaO0.13%0.002
CaO10.43%0.539
Li2O0.36%0.035
MgO0.51%0.037
K2O2.17%0.067
Na2O3.40%0.159
SrO3.81%0.107
PbO4.24%0.055
Al2O37.06%0.201
B2O38.98%0.374
SiO258.80%2.835
Oxide Weight289.41
Formula Weight289.41
If this formula is not unified correctly please contact us.
COLE - Co-efficient of Linear Expansion 7.6 x 10-6
GSPT - Frit Softening Point 1600F

Out Bound Links


By Tony Hansen

XML for Import into INSIGHT

<?xml version="1.0" encoding="UTF-8"?> <material name="Hommel Frit 486" descrip="Calcium strontium borosilicate frit" searchkey="" loi="0.00" casnumber="65997-18-4"> <oxides> <oxide symbol="BaO" name="Barium Oxide, Baria" status="" percent="0.130" tolerance=""/> <oxide symbol="CaO" name="Calcium Oxide, Calcia" status="" percent="10.430" tolerance=""/> <oxide symbol="Li2O" name="Lithium Oxide, Lithia" status="" percent="0.360" tolerance=""/> <oxide symbol="MgO" name="Magnesium Oxide, Magnesia" status="" percent="0.510" tolerance=""/> <oxide symbol="K2O" name="Potassium Oxide" status="" percent="2.170" tolerance=""/> <oxide symbol="Na2O" name="Sodium Oxide, Soda" status="" percent="3.400" tolerance=""/> <oxide symbol="SrO" name="Strontium Oxide, Strontia" status="" percent="3.810" tolerance=""/> <oxide symbol="PbO" name="Lead Oxide" status="" percent="4.240" tolerance=""/> <oxide symbol="Al2O3" name="Aluminum Oxide, Alumina" status="" percent="7.060" tolerance=""/> <oxide symbol="B2O3" name="Boric Oxide" status="" percent="8.980" tolerance=""/> <oxide symbol="SiO2" name="Silicon Dioxide, Silica" status="" percent="58.800" tolerance=""/> </oxides> </material>


Feedback, Suggestions

Your email address

Subject

Your Name

Message


Copyright 2003, 2008, 2015 https://digitalfire.com, All Rights Reserved